AI-Driven Superalloy Design: Language Models Learn from Physics
Published:Nov 15, 2025 05:08
•1 min read
•ArXiv
Analysis
This research explores a novel application of language models, utilizing physics-based feedback to refine their ability to design complex materials. The study's focus on superalloys indicates a potential for significant advancements in material science and engineering.
Key Takeaways
Reference
“The study focuses on tuning language models to design BCC/B2 superalloys.”